Export Packaging Requirements: What to Specify to a Chinese Factory

17 minute readUpdated 24/11/2026

Short answer Specify the board grade (wall type and ECT), a minimum compression strength for the bottom carton, and an ISTA 1A or 2A drop test. Add ISPM 15 heat-treated pallets, desiccants for long sea routes, inner cushioning for fragile goods, and a written packaging clause with photos before the balance.

Key takeaways

  • Board grade is a number, not a word: Amazon's box spec for inbound shipments lists B flute, ECT-32 and 200 lb burst strength.

  • Humidity kills stacking strength: above 95.00% relative humidity, a carton can lose more than 60.00% of its stacking strength.

  • Stack pattern matters too: interlocked stacks lost 49.00% to 54.00% of compression strength in a Fibre Box Association study.

  • Three ISTA tests cover most orders: 1A screens packages up to 68 kg, 2A adds partial simulation, 3A simulates parcel delivery.

  • Wood pallets need treatment: ISPM 15 heat treatment means at least 56 °C at the wood core for 30 minutes.

Written by TRG Editorial Team · reviewed by importers

Reviewed by people who import from China every month. Every fee and rule is checked on the official page, last on 24/11/2026. How we check figures

Some links on this page are affiliate links. We may earn a commission at no extra cost to you. It never changes our ranking. How we make money

Your factory says the goods will be packed in "strong export cartons". That phrase means nothing on a damage claim. This guide turns export packaging requirements into numbers a Chinese supplier can follow, test and sign.

Diagram of five nested export packaging layers, unit pack to container, with the risk each controlsExport packaging: five layers, five risksEach layer has its own line in your packaging specificationunitinner packcushioncartonpalletcontainer1Unit packpoly bag, sachetscratches, rust2Inner packcushion, dividersshock, vibration3Master cartonboard grade, ECTcrushing in a stack4PalletISPM 15 or plasticborder rejection5Containerdry load, desiccantcontainer rain
five layers of protection between the factory and your warehouse

Most advice stops at "use double-wall boxes". The real questions are harder: how strong must the bottom carton be, and which test fits your route? You get board grades, a strength estimate, tests, a moisture plan and a clause for your order.

Export packaging requirements at a glance

No single law sets carton strength. Physics sets what a stack can carry. Carriers and marketplaces set minimum grades, plant health rules cover wood, and your contract decides who pays for breakage.

The US government's export guidance names four classic problems: breakage, moisture, pilferage and excess weight. It notes that air shipments usually need lighter packing than ocean shipments.

RequirementWhat to specify
Board gradeSingle or double wall, flute, ECT or burst value
Stacking strengthMinimum box compression (BCT) for the bottom carton
Transit testISTA 1A, 2A or 3A, or a drop test at inspection
PalletsISPM 15 stamp on solid wood, or plastic, paper or plywood
MoistureDry loading, desiccant bags, humidity cards, liners
Inner packingCushion thickness, dividers, allowed materials
Marks and labelsMain mark, side mark, symbols, barcodes

Marks, ISO 780 symbols and barcodes are covered in our guide to shipping marks and carton labels. This guide focuses on whether the carton survives. Use the tree below to choose a packing level.

Decision tree choosing carton grade and ISTA test by route, stack load and fragilityWhich packing level and test?A starting point; confirm the grade with the strength estimate later in this guide1. Will cartons travel by parcel or to FBA?courier, Amazon, e-commerceParcel level: min. 32 ECT, B flutetest: ISTA 3A (or ISTA 6-Amazon)yesno2. Is the stack high or the carton heavy?floor-loaded container, long storageDouble wall (5-layer), BCT targetcalculate the bottom-carton loadyesno3. Is the product fragile or high value?glass, ceramics, electronicsAdd inner cushioning + ISTA 2Aconditioning, compression, vibration, shockyesnoSingle wall (3-layer) can workscreen with ISTA 1A, recheck at inspection
which packing level and test does your shipment need?

The tree is a starting point, not a rule. Write the result into your product specification sheet, so the packing becomes part of the order.

Corrugated board grades: single, double and triple wall

Corrugated board is paper glued in layers. Flat sheets called liners sit on each side of a wavy sheet called the fluting. GWP, a UK packaging maker, describes single wall as two liners and one layer of fluting. Double wall adds a second fluting and liner. Triple wall adds one more.

Chinese factories count the paper sheets instead. Single wall is "3-layer" (三层), double wall is "5-layer" (五层) and triple wall is "7-layer" (七层). Use both names in your order to avoid confusion.

The flute size changes thickness and behaviour. GWP gives typical thicknesses. B flute is about 3 mm and C flute 3.5 to 4 mm. A flute is 5 mm and E flute 1 to 1.5 mm. A BC double wall is 6 to 7 mm.

DS Smith, a large board maker, calls B flute the most widely specified profile. C flute gives more compression strength but crushes more easily. BC double wall is chosen when stacking strength is important.

Cross-sections of single, double and triple wall corrugated board with Chinese layer namesCorrugated board: single, double and triple wallLiners (black lines) and fluting (waves). Chinese factories count the paper layersSingle wall3-layer (三层)2 liners + 1 flutingB flute about 3 mmC flute 3.5 to 4 mmlight and medium cartonsDouble wall5-layer (五层)3 liners + 2 flutingsBC flute 6 to 7 mmchosen when stackingstrength is importantTriple wall7-layer (七层)4 liners + 3 flutingsheavy or large itemslarge export cartonsSources: GWP (thickness, layers), DS Smith (uses). Thickness values are typical, not guaranteed.
cross-sections of single, double and triple wall board

China has its own national standard for transport cartons. GB/T 6543-2025 covers single and double corrugated boxes for transport packages. The State Administration for Market Regulation lists it as current from 01/12/2025. It replaced the 2008 edition.

A Code of China summary says it covers contents up to 55 kg (indicative). Quoting the number gives inspectors a reference.

Never accept "export carton" alone. Write "5-layer BC double wall, minimum 48 ECT", or your calculated grade, and ask for it printed on the bottom flap.

ECT, BCT and burst: what each carton number tells you

Three tests appear on carton quotes. Buyers often mix them up.

1. Burst strength (Mullen test)

A rubber membrane is pushed into the board until it breaks. It measures puncture resistance. ISO 2759:2014 covers boards from 350 kPa to 5,500 kPa. US tables quote lb per square inch, such as "200 lb test".

2. Edge crush test (ECT)

ECT crushes a small strip of board on its edge. It predicts how well box walls carry a top load. The ISO method is ISO 3037:2022. Results are in kN/m, or lb per inch, such as "32 ECT".

3. Box compression test (BCT)

BCT crushes a whole box between two plates, using methods such as ASTM D642. BCT is the number that matters for stacking, because it includes box size and construction.

Comparison cards for burst, edge crush and box compression tests with their standardsThree carton numbers, three different questionsSpecify ECT for the board and BCT for the finished, stacked boxBurst (Mullen)ISO 2759:2014membrane pushed throughthe board until it breaksunit: kPa or lb/sq intells you: puncture andrough handling resistanceEdge crush (ECT)ISO 3037:2022board strip crushedon its edgeunit: kN/m or lb/intells you: how well thewalls carry a top loadBox compression (BCT)ASTM D642whole box crushedbetween two platesunit: kgf, N or lbtells you: the stackingload before failureExample grades: "200 lb test" is a burst value; "32 ECT" is an edge crush value. Amazon lists both.Sources: ISO, ASTM (checked 24/11/2026); Amazon Seller Central shipping requirements
burst, ECT and BCT compared

The US carrier table, known as Item 222 or Rule 41, links each grade to a maximum box weight. iPack, a packaging supplier, publishes it. A single-wall box at 32 ECT or 200 lb burst is rated for 65 lb, or 29.48 kg. A double-wall box at 42 ECT is rated for 80 lb (36.29 kg), and at 48 ECT for 100 lb (45.36 kg).

Those ratings cover handling a single box, not the bottom of a stack. For stacking you need a BCT target, which the next section estimates.

Fees and rules change often. Get the TRG Importer Brief: one short email a week with changes that affect importers.

Estimating carton strength with the McKee formula

In 1963, McKee published an equation that links ECT to box compression. Researchers at the US Forest Products Laboratory call it the state of the art among most industry estimates. They also call it a simplification with many constraints. Treat its result as an approximation.

The simplified form, as published by AICC, the US association of independent box makers, is shown below.

BCT (lb) = 5.87 × ECT (lb/in) × √(board caliper in inches × box perimeter in inches).

The perimeter is twice the length plus twice the width. The caliper is the board thickness. Georgia Tech labels this version "easy but not accurate".

Here is what this means in practice. Take a carton of 60 × 40 cm. Its perimeter is 200 cm, or 78.74 inches. A 32 ECT single wall in B flute (3 mm, 0.1181 in) gives about 572.84 lb. That is about 259.83 kg of top load in lab conditions.

Bar chart of McKee box compression estimates for four board grades against required loadsEstimated box compression, 60 × 40 cm carton (kg)Simplified McKee formula, lab conditions. Approximation only: confirm with a BCT test010020030040050060032 ECT, B flute single wall259.8332 ECT, C flute single wall300.0344 ECT, C flute single wall412.5448 ECT, BC double wall573.70- - 250.00 kg needed, columns + humid sea leg- - 434.78 kg needed, interlocked + humidRequired loads from the worked example below (80.00 kg on the bottom carton). Formula: simplified McKee, per AICC.
McKee estimates for a 60 × 40 cm carton (approximation)

The same footprint in 44 ECT C flute gives about 412.54 kg. A 48 ECT BC double wall reaches about 573.70 kg. These are lab values. Board is usually tested at 50.00% relative humidity, while cartons at sea often face up to 90.00%. Real containers are harsher, so the next step is to reduce them.

📌 Note: The McKee estimate assumes a regular slotted carton that is empty and well made. Dividers, handholes, vent holes and printed panels change the result. For a high-value product, pay for a real BCT test on filled samples.

Pallets, stacking and ISPM 15 inside the container

A carton's lab strength shrinks in real use. Three factors cut it: how you stack, how humid it gets and how long the load sits. Each one is a multiplier on the BCT.

The stacking pattern comes first. A Fibre Box Association study tested pallet patterns in 2021. Columnar aligned stacks, corner on corner, lost 12.00% to 20.00% of strength. A 0.75 inch misalignment cost 44.00% to 45.00%. Interlocked stacks lost 49.00% to 54.00%.

Top views of columnar, misaligned and interlocked pallet patterns with strength lostStacking pattern vs compression strength lostTop view: filled boxes = lower layer, dashed = layer above. Loss vs a single boxColumnar alignedcorner on cornerstrength lost12.00% to 20.00%Misaligned 0.75 incolumns shiftedstrength lost44.00% to 45.00%Interlockedrows turned 90°strength lost49.00% to 54.00%Source: Fibre Box Association pallet patterns study (32 and 44 ECT boxes). Bars show the top of each range.
how the pallet pattern cuts compression strength

Humidity comes second. An NMFTA article citing the Fibre Box Handbook gives a stark figure. Above 95.00% relative humidity, stacking strength can fall by more than 60.00%. Liquid water is worse: paper packaging can lose over 90.00% of its strength on contact. The same article notes that corners carry about two thirds of the load.

Time under load is the third factor. No primary source we checked gave one number, so keep a margin.

Ask the factory to stack columns, corner on corner, with no overhang past the pallet edge. Cartons on a 600 × 400 mm module fill standard pallets cleanly. Our guide to container dimensions and loading capacity shows how many pallets and cartons fit.

Wood pallets bring a legal rule. ISPM 15, the IPPC standard on wood packaging, requires solid wood to be treated and marked. The IPPC review of heat treatment states the schedule: a core temperature of at least 56 °C for at least 30 minutes. How to read the stamp is covered in our guide to carton marks and the ISPM 15 stamp.

US CBP excludes manufactured wood, pieces under 6 mm thick and paper. Plastic, paper or plywood pallets avoid the stamp issue.

Drop and vibration tests: ISTA 1A, 2A and 3A

Drops and vibration need a test. The International Safe Transit Association (ISTA) groups its procedures in series by how closely they simulate real transport.

1. ISTA 1 series: integrity tests

ISTA calls the 1 series non-simulation tests. They challenge the strength of the product and package together. ISTA 1A covers packages of 68 kg or less; 1B covers heavier ones. ISTA says 1A is not designed to simulate real transport, so use it as a screen.

2. ISTA 2 series: partial simulation

The 2 series adds at least one element of a full simulation. ISTA 2A covers single packages of 68 kg or less. Micom, a test lab, lists its sequence: atmospheric conditioning, compression, vibration, shock, then vibration again. The compression step makes 2A useful for sea cartons that will be stacked.

3. ISTA 3 series: general simulation

ISTA 3A simulates parcel delivery for packages up to 70 kg. Micom lists 17 drops in two blocks, plus random vibration, with heights set by weight. ISTA 3E covers unitised loads, such as a pallet of similar cartons going by truck to one destination.

4. ISTA 6 series: retailer tests

The 6 series reflects large retailers and carriers. ISTA 6-Amazon.com-SIOC is a general simulation for products shipped to Amazon fulfilment centres. It applies to items sold in their own container, without an Amazon overbox.

ISTA test series 1, 2, 3 and 6 from screening to full simulationISTA test series: from screening to full simulationCloser to real transport as you move right; cost and time rise tooscreeningclosest to the real supply chain1 seriesIntegrity tests1A: up to 68 kg1B: over 68 kgnot a transportsimulationUse for:first screen ofa new carton2 seriesPartial simulation2A: up to 68 kgconditioning,compression,vibration, shockUse for:stacked sea cartons,fragile goods3 seriesGeneral simulation3A: parcel, to 70 kg,17 drops + vibration3E: unitised loadsby full truckUse for:parcel ande-commerce6 seriesRetailer tests6-Amazon.com-SIOC:item ships in itsown box to Amazonfulfilment centresUse for:selling on Amazonwithout an overboxSources: ISTA test procedures; Micom lab pages for the 2A sequence and 3A drop count (checked 24/11/2026)
the ISTA series, from screening to full simulation

A simple rule: use ISTA 1A to screen a new carton, 2A for fragile sea cartons and 3A when the carton later travels by parcel.

For repeat orders, add a carton drop test to the pre-shipment inspection. It does not replace ISTA, but it catches weaker board on a later batch.

Moisture control: container rain, desiccants and humidity cards

A closed steel container heats in the sun and cools at night. Water vapour then condenses on the cold steel. This is called container rain, because drops fall onto the top cartons.

TIS, the German insurers' transport information service, explains the cycle. Condensation is worst on container ceilings. At about 25 °C outside, air in a brown-painted container can reach about 50 °C. A white container reaches about 38 °C.

TIS names the cargo, its packaging and the wooden floor as the largest water sources. Dry loading matters most.

The CTU Code, the IMO, ILO and UNECE packing code, confirms the risk. It notes that standard containers allow only restricted air changes; their vents barely exchange air.

Container cross-section showing container rain and four moisture controlsContainer rain: how it forms and how to stop itDay: sun heats the steel and moisture leaves the cargo. Night: the ceiling cools and water drips downday: about 50 °C inside a brown boxat about 25 °C outside (TIS)cold ceiling at nighttop layer gets wet firstlargest water sources: cargo, packaging, wooden floor (TIS)1Load drydry pallets, indoor cartons, dry floor photo2Hang desiccant bagsmaker suggests 3 per 20 ft, 6 per 40 ft (indicative)3Humidity indicator cardspots turn blue to pink at 10.00% to 60.00% RH4Protect the unitsealed bag + silica gel for metal and electronics
how container rain forms, and four ways to stop it

1. Load dry

Ask for dry pallets and cartons stored indoors. Do not load in rain. Ask for a photo of the dry, empty container floor.

2. Hang container desiccants

Container desiccants are bags of calcium chloride that trap water. AGM, a US maker, says its Container Dri II traps up to 150.00% of its weight in moisture. It suggests 3 bags for a 20 ft container and 6 for a 40 ft. Treat the count as indicative; longer and hotter voyages need more.

3. Add humidity indicator cards

A humidity indicator card shows relative humidity with colour spots. The card in the Médecins Sans Frontières catalogue has spots from 10.00% to 60.00%. Each turns from blue to pink when its level is reached. Put one card in a few sample cartons and photograph it on arrival.

4. Protect the product itself

For metal parts and electronics, use sealed poly bags with small silica gel sachets inside the unit pack.

Inner packaging for fragile goods and Amazon FBA basics

Inner packaging fights shock and vibration. It stops each unit moving or touching the carton wall.

Amazon publishes clear minimums, and they are useful even if you never sell there. Its shipping requirements list four box items: a regular slotted carton, B flute, ECT-32 and 200 lb per square inch burst strength. The list gives no "and" or "or"; in the carrier table both ratings describe the same single-wall class. It asks for at least 2 inches (5.08 cm) of packing around each item and the box walls. That rule falls away for a manufacturer's case pack.

Amazon also lists materials. Bubble wrap, full sheets of kraft paper, air pillows and polyethylene foam sheets are allowed. Packing peanuts of any type, foam strips, crinkle wrap and shredded paper are banned. Its test is simple: shake the packed box gently, and nothing should move.

Carton cross-section with 2 inches of cushioning and Amazon allowed and banned materialsInner packing: keep every unit stillAmazon's minimums are a good default even outside Amazonfragile unitin a sealed bag2 in2 in (5.08 cm)cushion on every sideAllowed✓ bubble wrap✓ full sheets of kraft paper✓ inflatable air pillows✓ polyethylene foam sheetshake test: nothingmoves inside the boxNot allowed✕ packing peanuts (all)✕ foam strips✕ crinkle wrap✕ shredded paper✕ thermocol chips✕ StyrofoamSource: Amazon Seller Central shipping and routing requirements. Not needed for a manufacturer case pack.
inner packing for a fragile unit, using Amazon's minimums

A standard Amazon box must not exceed 50 lb (22.68 kg) unless it holds one heavier item. Packaging guides report a multi-item limit of 36 × 25 × 25 inches since 20/06/2025 (indicative); check Seller Central before you pack.

Outside Amazon, specify the cushion type, its thickness and any dividers or moulded pulp trays. Our guide to shipping from China to Amazon FBA covers labels, pallets and fees.

Worked example: specifying a carton for a 40 ft high cube

Example: a Jeddah importer orders ceramic mugs. Each carton is 60 × 40 × 40 cm and 16.00 kg gross, floor-loaded in a 40 ft high cube.

Hapag-Lloyd gives the inside height of a 40 ft high cube as 2,700 mm. That fits six layers of 400 mm cartons. The bottom carton then carries five cartons above it.

LineCalculationResult
Layers that fit2,700 mm ÷ 400 mm, rounded down6 layers
Load on the bottom carton5 cartons × 16.00 kg80.00 kg
Stacking factor, columnar1.00 − 0.20 (worst of 12.00% to 20.00% loss)0.80
Humidity factor1.00 − 0.60 (loss above 95.00% RH)0.40
Required BCT, columnar80.00 ÷ (0.80 × 0.40) = 80.00 ÷ 0.32250.00 kg
Stacking factor, interlocked1.00 − 0.54 (worst of 49.00% to 54.00% loss)0.46
Required BCT, interlocked80.00 ÷ (0.46 × 0.40) = 80.00 ÷ 0.184434.78 kg
32 ECT B flute (McKee)5.87 × 32 × √((3 ÷ 25.4) × 78.74) = 572.84 lb259.83 kg
48 ECT BC double wall (McKee)5.87 × 48 × √((6.5 ÷ 25.4) × 78.74) = 1,264.79 lb573.70 kg

The single wall passes the columnar case by less than 10.00 kg. It fails if workers interlock the stack. The double wall gives room for both patterns and for time under load, which the table leaves out.

Step chart from an 80.00 kg top load to 250.00 kg and 434.78 kg required box compressionExample: from top load to the BCT you specify (kg)Ceramic mugs, 16.00 kg cartons, 6 layers in a 40 ft high cube. Planning factors, approximation onlycolumns: 250.00interlocked: 434.7880.00top loadon bottom carton100.00÷ 0.80columns250.00÷ 0.40humidity173.91÷ 0.46interlocked434.78÷ 0.40humidity573.7048 ECT BCMcKee32 ECT B flute single wall estimate: 259.83 kg. It passes columns narrowly and fails interlocked stacking.Time under load is not included: keep a margin and confirm with a lab BCT test.
example: from an 80.00 kg top load to the BCT you specify

The importer specifies "5-layer BC double wall, minimum 48 ECT, BCT at least 435.00 kg, columns only". The factors are rounded planning values, not a standard. Treat the result as an approximation and confirm it with a lab BCT test.

Our guide to cargo insurance for China imports explains why insurers can refuse claims for insufficient packing.

Packaging spec clause and checklist for your supplier

A clause turns the numbers into a duty. Put it in the purchase order and ask the supplier to sign it.

Packaging clause (template): "Outer cartons: 5-layer BC double wall, minimum 48 ECT, BCT at least 435.00 kg, per GB/T 6543-2025. Maximum 16.00 kg gross per carton. Inner pack: each unit in a PE bag and a moulded pulp tray, no movement when shaken. Cartons stacked in columns, no overhang. Pallets, if used: ISPM 15 HT stamped, or plastic. Desiccant: 6 bags per 40 ft container. Drop test: ISTA 1A on 2 cartons before mass packing. Photos of open carton, sealed carton, stamp and loaded container sent before balance payment. Failed packing is repacked at the supplier's cost."

Mock packaging specification sheet with six annotated clause blocksAnatomy of a packaging clauseFictional purchase order annex. Each block is one testable linePackaging specification · PO 2026-118 (example)Outer carton5-layer BC, 48 ECT, BCT ≥ 435.00 kg1grade + test valueWeight capmax 16.00 kg gross per carton2protects the stackInner packPE bag + pulp tray, no movement3shock and vibrationPallets / stackingISPM 15 HT or plastic; columns4border + strengthMoisture6 desiccant bags per 40 ft5container rainProof + remedyISTA 1A, photos, repack at cost6enforceable dutySigned by supplier · date DD/MM/YYYY
anatomy of a packaging clause: six blocks

Add packing checks to the inspection booking: grade print, gross weight, inner pack and a drop test. Our explainer on AQL sampling tables shows how many cartons the inspector should open.

Export packaging checklist before mass packing

For the full order process around this checklist, see our step-by-step guide on how to import from China.

What goes wrong in practice (and how to fix it)

1. The board gets weaker on repeat orders

The third order arrives in thinner board from a cheaper box maker. Fix: write the grade into the contract and check the flap stamp at every inspection.

2. Damp cartons go into the container

Cartons stored outdoors absorb water and leave China already weak. Fix: ask for indoor storage, a dry container floor photo and desiccant bags for long routes.

3. Workers interlock the stack

Interlocking looks stable but can halve compression strength. Fix: write "columns only" in the loading instructions and ask for photos.

4. The pallet is rejected at the border

A missing or unreadable ISPM 15 stamp can lead to rejection or destruction of the wood. GOV.UK states this for Great Britain. Fix: ask for a stamp photo, or use plastic pallets.

5. Damage is found but the claim fails

Insurers ask whether packing was adequate. Fix: keep the signed clause, test reports and loading photos, and note damage on the delivery receipt.

📌 Note: If cartons arrive crushed, photograph the doors, the stack and each damaged carton before moving anything. Notify the carrier and insurer in writing, and keep a few damaged cartons as evidence.

By region: MENA, Europe/UK, USA

MENA. USDA APHIS lists Egypt, Jordan, Lebanon and Oman among countries requiring ISPM 15. The list is not complete, so check Gulf ports with your forwarder. Summer heat in Gulf ports makes dry loading and desiccants more important.

Europe and UK. Both apply ISPM 15 to solid wood packaging, as our shipping marks guide explains. The EU Packaging and Packaging Waste Regulation (EU) 2025/40 applies from 12/08/2026. The European Commission says its labelling rules follow in 2028 and limits on empty space in 2030.

USA. USDA APHIS sets the wood packaging rules. No federal law sets carton strength; carrier tables and Amazon rules act as the market standard.

Glossary

Flute: the wavy paper layer between flat liners; B, C, A and E differ in height.

ECT: edge crush test, the board's resistance to crushing on its edge.

BCT: box compression test, the load at which a whole box fails.

Burst test: the pressure needed to puncture the board.

McKee formula: an approximate equation estimating BCT from ECT, caliper and perimeter.

ISTA: International Safe Transit Association, publisher of package tests.

ISPM 15: the IPPC standard for treating and marking wood packaging.

Container rain: condensation dripping from a container ceiling onto cargo.

FAQ

What are the basic export packaging requirements?

A board grade strong enough for the stack, inner cushioning, moisture protection and correct marks. Wood pallets must meet ISPM 15.

Is single wall or double wall better for sea freight?

Double wall is safer for high or heavy stacks. If a single wall passes your BCT estimate only narrowly, choose double wall.

What does 32 ECT mean?

The board resists 32 lb per inch of edge before crushing. It says nothing about box size, so check BCT for stacking.

Is the McKee formula accurate?

No, it is an approximation for empty regular slotted cartons. Use it to choose a grade, then confirm with a lab test.

Which ISTA test should I ask a Chinese factory for?

ISTA 1A for basic screening, 2A for fragile sea cartons, and 3A if the carton travels by parcel.

Do plastic pallets need an ISPM 15 stamp?

No. ISPM 15 covers solid wood packaging only.

How many desiccant bags does a container need?

One maker suggests 3 bags for a 20 ft container and 6 for a 40 ft. Treat this as indicative; long, hot voyages need more.

Can a pre-shipment inspection check packaging?

Yes. Ask the inspector to check grade print, gross weight, inner pack and a drop test.

Sources

32 official and provider pages, each with the date we checked it